Abstract
Current systems for photogrammetry analysis rely mainly on two-dimensional visualization methods, particularly Scanning Electron Microscopy (SEM). The absence of three-dimensional information prevents the determination of important quantitative features such as local roughness and precludes a deeper comprehension of the failure mechanisms. This paper describes a new multi-scale stereo-photogrammetry system for inspection of fracture surfaces based on SEM images. The system facilitates the reconstruction of complete 3D fracture surfaces and provides interactive visualization of the multi-scale structure, thus offering better insight into fracture surfaces at different levels of detail. In particular, a new method has been developed for geometric reconstruction of a 3D textured mesh from SEM stereo images. The mesh is represented as a 3D geometric multi-resolution structure. The sampled images are represented in the form of a multi-scale hierarchical textured structure. Thus, the global shape of the sample is represented by a 3D mesh, while its micro details are represented by textured data. This multi-scale and hierarchical structure allows interactive multi-scale navigation of the 3D textured mesh. The Regions of Interest (ROI) can actually be inspected interactively at different scales by means of optical or digital zooming. Thus, the digital model can be visualized and the behavior of the 3D material can be analyzed interactively. The contributions of this research include: (a) a new 3D multi-scale reconstruction method for SEM stereo images; (b) a new visualization module for multi-scale inspection, modeling and analysis of micro-structures for a variety of materials; and (c) 3D insight into and better understanding of fracture phenomena for material micro-structures. The feasibility of the proposed method is demonstrated on samples of different materials, and a performance analysis is applied on the resulting multi-scale model. The roughness calculation was verified against roughness calculation applied to the optical profilometer.
| Original language | English |
|---|---|
| Pages (from-to) | 975-991 |
| Number of pages | 17 |
| Journal | Experimental Mechanics |
| Volume | 52 |
| Issue number | 8 |
| DOIs | |
| State | Published - Oct 2012 |
Keywords
- Fracture surfaces
- Multi-resolution
- Multi-scale
- Stereo-photogrammetry
- Textured meshes
- Visualization analysis
All Science Journal Classification (ASJC) codes
- Aerospace Engineering
- Mechanics of Materials
- Mechanical Engineering