This work continues our systematic study of Li-and Mn-rich cathodes for lithium-ion batteries. We chose Li2MnO3 as a model electrode material with the aim of correlating the improved electrochemical characteristics of these cathodes initially activated at 0°C with the structural evolution of Li2MnO3, oxygen loss, formation of per-oxo like species (O22−) and the surface chemistry. It was established that performing a few initial charge/discharge (activation) cycles of Li2MnO3 at 0°C resulted in increased discharge capacity and higher capacity retention, and decreased and substantially stabilized the voltage hysteresis upon subsequent cycling at 30°C or at 45°C. In contrast to the activation of Li2MnO3 at these higher temperatures, Li2MnO3 underwent step-by-step activation at 0°C, providing a stepwise traversing of the voltage plateau at >4.5 V during initial cycling. Importantly, these findings agree well with our previous studies on the activation at 0°C of 0.35Li2MnO3·0.65Li[Mn0.45Ni0.35Co0.20]O2 materials. The stability of the interface developed at 0°C can be ascribed to the reduced interactions of the per-oxo-like species formed and the oxygen released from Li2MnO3 with solvents in ethylene carbonate–methyl-ethyl carbonate/LiPF6 solutions. Our TEM studies revealed that typically, upon initial cycling both at 0°C and 30°C, Li2MnO3 underwent partial structural layered-to-spinel (Li2Mn2O4) transition.
Original language | English |
---|---|
Article number | 4388 |
Pages (from-to) | 1-22 |
Number of pages | 22 |
Journal | Materials |
Volume | 13 |
Issue number | 19 |
DOIs | |
State | Published - 1 Oct 2020 |
Keywords
- Bulk and surface characteristics
- Decreased the voltage hysteresis
- Layered-to-spinel transition
- Li-and Mn-rich materials
- LiMnO activation at 0°C
- Lithium-ion batteries
- Stabilized cycling
All Science Journal Classification (ASJC) codes
- General Materials Science
- Condensed Matter Physics