Atomic Layer Deposition for Gradient Surface Modification and Controlled Hydrophilization of Ultrafiltration Polymer Membranes

Tamar Itzhak, Naama Segev-Mark, Assaf Simon, Volker Abetz, Guy Z. Ramon, Tamar Segal-Peretz

Research output: Contribution to journalArticlepeer-review

Abstract

In recent years, atomic layer deposition (ALD) has emerged as a powerful technique for polymeric membrane surface modification. In this research, we study Al2O3 growth via ALD on two polymeric phase-inverted membranes: polyacrylonitrile (PAN) and polyetherimide (PEI). We demonstrate that Al2O3 can easily be grown on both membranes with as little as 10 ALD cycles. We investigate the formation of Al2O3 layer gradient through the depth of the membranes using high-resolution transmission electron microscopy and elemental analysis, showing that at short exposure times, Al2O3 accumulates at the top of the membrane, reducing pore size and creating a strong growth gradient, while at long exposure time, more homogeneous growth occurs. This detailed characterization creates the knowledge necessary for controlling the deposition gradient and achieving an efficient growth with minimum pore clogging. By tuning the Al2O3 exposure time and cycles, we demonstrate control over the Al2O3 depth gradient and membranes' pore size, hydrophilicity, and permeability. The oil antifouling performance of membranes is investigated using in situ confocal imaging during flow. This characterization technique reveals that Al2O3 surface modification reduces oil droplet surface coverage.

Original languageEnglish
Pages (from-to)15591-15600
Number of pages10
JournalACS Applied Materials and Interfaces
Volume13
Issue number13
DOIs
StatePublished - 7 Apr 2021

Keywords

  • atomic layer deposition
  • gradient
  • membranes
  • oxide
  • transmission electron microscopy
  • ultrafiltration