Abstract
Designing high voltage (>3 V) and stable electrochemical supercapacitors with low self-discharge is desirable for the applications in modern electronic devices. This work demonstrates a 4 V symmetric supercapacitor with stabilized cycling performance through atomic layer deposition (ALD) of alumina (Al2O3) on the surface of activated carbon (AC). The 20-cycle ALD Al2O3 coated AC delivers 84 % capacitance retention after 1000 charge/discharge cycles under 4 V, contrary to the bare AC cells having only 48 % retention. The extended cycling life is associated with the thickened Stern layer and suppressed oxygen functional group. The self-discharge data also show that the Al2O3 coating enables AC cells to maintain 53 % of charge retention after 12 h, which is more than twice higher than that of bare AC cells under the same test protocol of 4 V charging. The curve fitting analysis reveals that ALD coating induced slow self-discharge dominated by ion diffusion mechanism, thus enhancing the AC surface energy.
| Original language | English |
|---|---|
| Pages (from-to) | 402-407 |
| Number of pages | 6 |
| Journal | ChemistryOpen |
| Volume | 10 |
| Issue number | 4 |
| DOIs | |
| State | Published - Apr 2021 |
Keywords
- activated carbon
- atomic layer deposition
- high voltage
- self-discharge
- supercapacitors
All Science Journal Classification (ASJC) codes
- General Chemistry